Cobalt chrome non precious dental alloys for frames ingot, partial denture
Our dental cobalt chrome alloy for partial denture frames has a strong resistance to traction and excellent workability. It enables to obtain smooth and compact surfaces and reduce the oxide formation. They are an economical alternative to Gold & Silver based alloys (precious) but perform well due to their mechanical properties and biocompatibility.
Chemical Composition:
Co: 60%
Cr: 30%
Mo: 9%
Others: 1%
Melting range: 1175-1350C
VHN: 380HV10
Density: 8.5cm³
Advantages:
(1).Superior mechanical performance castability, toughness
(2).Corrosion resistance , wear resistance , high intensity , high hardness, stays in shape
(3).Nickle-free &beryllium-free, great biocompatibility
FAQ:
What is the perfect temperature to obtain the best result when casting?
The casting temperature should always maintain 100~150℃ higher than liquidus temperature.
What is the perfect timing to obtain the best result when casting?
While casting Nickel Chrome alloys that don't contain Beryllium, the surface of the melting alloys will appear a layer of shadow. Once the shadow disappears and the edges of the alloy have become rounded (melted until it becomes a sphere shape is not necessary) will be the best timing for casting. Perfect timing for casting Cobalt Chrome alloy is to heat it till the surface membrane perforated and a spark of bright light start to appear.
Cobalt Chrome casting piece is incomplete, what are the causes?
1. Casting ring is not heated evenly: While casting Cobalt alloys, casting ring must heat up gradually and slowly before reaches 300℃. Let it sit in the oven in between 300℃ and 600℃ for 10-30 minutes. Once it heats up to the desired temperature, maintain the same temperature for at least 30 minutes before casting.
2. Casting temperature is below/above alloy's requirement.
3. Strub designed improperly: For example, Strub is too narrow. We strongly recommend the Strub diameter consist of 5mm or more.
4. The amount of alloy is not enough for the casting piece or the centrifugal force of casting pressure is not enough.
5. Casting piece has not avoided the heat center.
![]() |